Everyone has their own preference for what they use. This is what I use:
AUSTOR 60-40 Tin Lead Rosin Core Solder Wire 0.8mm
CAIG RSF-R80-8G DeoxIT Rosin Soldering Flux Syringe 8g
Hyakol 99% Isopropyl Alcohol - 16 Oz
I personally solder at 400'c. You may not want to use that high of a temperature. The more heat, generally the faster you want to work.
AUSTOR 60-40 Tin Lead Rosin Core Solder Wire 0.8mm
CAIG RSF-R80-8G DeoxIT Rosin Soldering Flux Syringe 8g
Hyakol 99% Isopropyl Alcohol - 16 Oz
I personally solder at 400'c. You may not want to use that high of a temperature. The more heat, generally the faster you want to work.